Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 cm/cm @Thickness 3.17 mm |
0.00200 in/in @Thickness 0.125 in |
ASTM D955 |
Oxford Polymers ABS 30GF-BK ABS, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: Pre-colo.. |
|||
Linear Mold Shrinkage | 0.00200 cm/cm | 0.00200 in/in | ASTM D955 |
Niche Polymer PA6GF43BK Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00200 cm/cm | 0.00200 in/in | ASTM D955 |
Niche Polymer PA6GF43N Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00200 - 0.0130 cm/cm | 0.00200 - 0.0130 in/in | Average value: 0.00513 cm/cm Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00404 cm/cm Grade Count:12 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00300 cm/cm | 0.00200 - 0.00300 in/in | Average value: 0.00267 cm/cm Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0114 cm/cm | 0.00200 - 0.0114 in/in | Average value: 0.00556 cm/cm Grade Count:81 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00671 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00552 cm/cm Grade Count:106 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00500 cm/cm | 0.00200 - 0.00500 in/in | Average value: 0.00350 cm/cm Grade Count:8 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0370 cm/cm | 0.00200 - 0.0370 in/in | Average value: 0.0129 cm/cm Grade Count:17 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00671 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0200 cm/cm | 0.00200 - 0.0200 in/in | Average value: 0.0118 cm/cm Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00693 cm/cm Grade Count:7 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0400 cm/cm | 0.00200 - 0.0400 in/in | Average value: 0.0180 cm/cm Grade Count:15 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0400 cm/cm | 0.00200 - 0.0400 in/in | Average value: 0.0160 cm/cm Grade Count:109 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0250 cm/cm | 0.00200 - 0.0250 in/in | Average value: 0.0118 cm/cm Grade Count:23 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00386 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:19 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00369 cm/cm Grade Count:24 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0120 cm/cm | 0.00200 - 0.0120 in/in | Average value: 0.00509 cm/cm Grade Count:21 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00767 cm/cm Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |