Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Polycarbonate, 30% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | ASTM D955 |
PolyOne Edgetek® PK-15CF-15GB/000 Polyetheretherketone (PEEK), Glass Bead, Carbon Fiber Reinforced
(discontin Description/Features:Carbon Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | ASTM D955 |
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0030 cm/cm | 0.0025 - 0.0030 in/in | ASTM D955 |
PolyOne Lubri-Tech™ PI-10CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0030 cm/cm | 0.00050 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | |
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynam.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0030 cm/cm | 0.00050 - 0.0030 in/in | ASTM D955 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
MRC Polymers EMAREXâ„¢ 300 GF33 Nylon 6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | ASTM D955 |
Techmer ES Plaslube® J-1/CF/15/TF/20 NAT PA66 |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm @Thickness 1.59 mm |
0.0020 - 0.0030 in/in @Thickness 0.0625 in |
ASTM D955 |
Plastics Group Polifil® GFPC-20 20% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ISO 2577 |
Polyram RamTough PZ307G6 Polycarbonate, 30% Glass Fiber, UV Stabilized 30% glass fiber reinforced polycarbonate, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm @Thickness 3.17 mm |
0.0020 - 0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ MP-20GF/15T Modified PPO - 20% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | ASTM D955 |
PolyOne Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |