Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | With Flow; ISO 2577 |
Polykemi AB SCANAMID 66 A53^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | With Flow; ISO 2577 |
Polykemi AB SCANAMID 66 A53^EM Nylon 66, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ASTM D955 |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Linear Mold Shrinkage | 0.016 - 0.024 cm/cm | 0.016 - 0.024 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 D Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, developed for dowels.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.016 cm/cm @Thickness 3.20 mm |
0.016 in/in @Thickness 0.126 in |
Flow |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Linear Mold Shrinkage | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | Asahi Chemical test |
Asahi Kasei Tenac®-C 4510 Acetal Copolymer, General Purpose
(discontinued **) General-purpose grade, characterized by balanced flowability and mechanical properties.Applications: Gears, cams, hose joints, clips, switches, mechanical parts of audio and video equipment.This pro.. |
|||
Linear Mold Shrinkage | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | Asahi Chemical test |
Asahi Kasei Tenac®-C 7510 Acetal Copolymer, High Flow
(discontinued **) High-flow grade, suited for thin-wall, long-flow-distance moldings.Applications: Lighters, aerosol bottles, fasteners.This product is not a part of the standard product line dated 2003. |
|||
Linear Mold Shrinkage | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | |
Lehmann & Voss LUVOCOM® 80/TF/18/GY Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Kolon KOCETAL® TC704 Mineral Reinforced Acetal Resin Whisker reinforced, improved wear and dimensional property. Applications: Dimensionally precise products. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Linear Mold Shrinkage | 0.016 - 0.019 cm/cm | 0.016 - 0.019 in/in | ASTM D955 |
Kolon KOPA® KN333HI5BL High Impact Nylon 66 Middle viscosity, Impact -resistantApplications A variety of fuse boxes, relax boxesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Global PPC-0320 Standard Grade Polypropylene Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Ineos 3950 Polypropylene Impact Copolymer Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1566L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
SK Chemicals SKYPEL G168D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | Borealis Method |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | |
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | 4 inch disk; ASTM D955 |
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | MD; ASTM D955 |
Aclo Accucomp Polyethylene LD0109L Low Density |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Buckeye Polymers BP Flex D5606 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM Data; MD |
BASF Ultramid® 1000-11 NF2001 PA66 (Conditioned) Ultramid 1000-11 NF2001 is a general purpose nylon 6/6. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Asahi Kasei Thermofil P-9900-0576 Unreinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 7606 UV NAT The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.016 cm/cm | 0.016 in/in | ASTM D955 |
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Linear Mold Shrinkage | 0.016 - 0.019 cm/cm | 0.016 - 0.019 in/in | ISO 2577 |
Polyram RamSter PF801 PBT, High Impact Modified High impact modified PBT for injection molding applications.Information provided by Polyram. |