Buckeye Polymers BP Flex D5606 TPO

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP Flex D5606 TPO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a wide service range from -20 degrees C to 120 degrees C, high tear resistance, low density, and good paintability.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Ultimate 17.9 MPa
2600 psi
ASTM D638
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D790
Tear Strength 91.2 kN/m
520 pli
ASTM D624