Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE ZS506 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ Nylon 6 Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
PolyOne Edgetek® PS-25MN/000 Polybutylene Terephthalate (PBT), Mineral Filled
(discontinued **) Description/Features:Mineral FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | |
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
ISO 294-4 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
Polyram PlusTek PB891 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Entec Hypro™ PP-HP12 Homopolymer, 12 Melt Flow This product in intended for general purpose injection molding applications such as caps and closures, resin furniture and consumer products.Information provided by Entec |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
E-Polymers TEKAMID® TB110HI , High Impact PA6, DAM High Impact resistance at low temperatureInformation provided by E-Polymers Co. Ltd. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | Bayer Test |
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Copolymer CP0437C10L Calcium Reinforced |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM Data; MD |
BASF Ultramid® A34 01 PA66 (Dry) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Ashley Polymers Ashlene® 626SB Nylon 6 Copolymer A flexible nylon copolymer, heat stabilized, in black, for tubing and other extrusion applications.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
Beijing Ranger Chem PBT 403 M-G0 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
Beijing Ranger Chem PBT-201-G0 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE ZS606 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
PolyOne Synprene® IT 36-018 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerGood Surface AppearanceOpaqueApplications:AutomotiveInteriorProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by P.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ISO 2577 |
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm | 0.014 - 0.023 in/in | ASTM D955 |
Samyang Tribit® 1800 PBT, High Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800 is a high viscosity grade.Information .. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm | 0.014 - 0.023 in/in | ASTM D955 |
Samyang Tribit® 1800H PBT, Extruding Formality Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800H is an extrusion grade.Information pro.. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
Beijing Ranger Chem PBT 403 M-G0 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |