Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00250 cm/cm Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Linear Mold Shrinkage | -0.00200 - 0.00400 cm/cm | -0.00200 - 0.00400 in/in | Average value: 0.00159 cm/cm Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Linear Mold Shrinkage | -0.00100 - 0.00400 cm/cm | -0.00100 - 0.00400 in/in | Average value: 0.000879 cm/cm Grade Count:42 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00400 cm/cm | 0.000 - 0.00400 in/in | Average value: 0.00126 cm/cm Grade Count:39 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00400 cm/cm | 0.000100 - 0.00400 in/in | Average value: 0.00183 cm/cm Grade Count:6 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00240 cm/cm Grade Count:5 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00400 cm/cm | 0.00200 - 0.00400 in/in | Average value: 0.00300 cm/cm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.00400 cm/cm | 0.000200 - 0.00400 in/in | Average value: 0.000985 cm/cm Grade Count:19 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00400 cm/cm | 0.000100 - 0.00400 in/in | Average value: 0.00150 cm/cm Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00333 cm/cm Grade Count:6 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00243 cm/cm Grade Count:5 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00400 cm/cm | 0.00200 - 0.00400 in/in | ASTM D955 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00204 cm/cm Grade Count:12 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage | 0.00280 - 0.00400 cm/cm @Temperature 80.0 - 80.0 °C |
0.00280 - 0.00400 in/in @Temperature 176 - 176 °F |
Average value: 0.00304 cm/cm Grade Count:20 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00400 cm/cm | 0.000500 - 0.00400 in/in | Average value: 0.00188 cm/cm Grade Count:28 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00225 cm/cm Grade Count:4 |
Overview of materials for Acrylic, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00240 cm/cm Grade Count:5 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00400 cm/cm | 0.00200 - 0.00400 in/in | ASTM D955 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |