Overview of materials for Acrylic, Glass Fiber Reinforced

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylic, Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.26 - 1.52 g/cc
0.0455 - 0.0549 lb/in³
Average value: 1.38 g/cc Grade Count:4
Filler Content 10.0 - 40.0 %
10.0 - 40.0 %
Average value: 25.0 % Grade Count:4
Water Absorption 0.200 - 0.300 %
0.200 - 0.300 %
Average value: 0.250 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00225 cm/cm Grade Count:4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.8 - 121 MPa
11000 - 17500 psi
Average value: 97.4 MPa Grade Count:4
Elongation at Break 1.00 %
1.00 %
Average value: 1.00 % Grade Count:4
Modulus of Elasticity 3.79 - 12.8 GPa
550 - 1850 ksi
Average value: 8.45 GPa Grade Count:4
Flexural Yield Strength 110 - 179 MPa
16000 - 26000 psi
Average value: 143 MPa Grade Count:4
Flexural Modulus 3.45 - 12.4 GPa
500 - 1800 ksi
Average value: 8.27 GPa Grade Count:4
Izod Impact, Notched 0.427 - 0.534 J/cm
0.800 - 1.00 ft-lb/in
Average value: 0.494 J/cm Grade Count:4
Izod Impact, Unnotched 1.60 - 2.14 J/cm
3.00 - 4.00 ft-lb/in
Average value: 1.80 J/cm Grade Count:4
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 - 102 °C
200 - 215 °F
Average value: 98.2 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 90.6 - 96.1 °C
195 - 205 °F
Average value: 93.3 °C Grade Count:4
Flammability, UL94 HB
HB
Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 - 1.00e+17 ohm-cm
1.00e+16 - 1.00e+17 ohm-cm
Average value: 7.75e+16 ohm-cm Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 177 - 210 °C
350 - 410 °F
Average value: 193 °C Grade Count:4
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Average value: 93.3 °C Grade Count:4
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:4