Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Epoxy Cure Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Overview of materials for Epoxy Cure Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.860 - 2.60 g/cc
0.0311 - 0.0939 lb/in³
Average value: 1.34 g/cc Grade Count:114
1.025 - 1.06 g/cc
<br>@Temperature 15.0 - 15.0 °C
0.03703 - 0.0383 lb/in³
<br>@Temperature 59.0 - 59.0 °F
Average value: 1.05 g/cc Grade Count:3
Water Absorption 0.0300 - 1.00 %
0.0300 - 1.00 %
Average value: 0.298 % Grade Count:25
Moisture Absorption at Equilibrium 2.80 - 9.40 %
2.80 - 9.40 %
Average value: 5.16 % Grade Count:7
Viscosity 0.650 - 1.20e+6 cP
0.650 - 1.20e+6 cP
Average value: 36500 cP Grade Count:102
15.0 - 78000 cP
<br>@Temperature 40.0 - 156 °C
15.0 - 78000 cP
<br>@Temperature 104 - 313 °F
Average value: 8950 cP Grade Count:4
Molecular Weight 158 - 1690 g/mol
158 - 1690 g/mol
Average value: 661 g/mol Grade Count:11
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00240 cm/cm Grade Count:5
Vapor Pressure 2.10e-8 - 0.0100 bar
0.0000158 - 7.50 torr
Average value: 0.00250 bar Grade Count:4
0.0100 - 0.0100 bar
<br>@Temperature 50.0 - 50.0 °C
7.50 - 7.50 torr
<br>@Temperature 122 - 122 °F
Average value: 0.00400 bar Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Shore D 50.0 - 95.0
50.0 - 95.0
Average value: 80.4 Grade Count:27
Tensile Strength, Ultimate 5.17 - 97.0 MPa
750 - 14100 psi
Average value: 33.7 MPa Grade Count:31
35.8527 - 35.8527 MPa
<br>@Temperature 149 - 149 °C
5200.01 - 5200.01 psi
<br>@Temperature 300 - 300 °F
Average value: 35.9 MPa Grade Count:1
Tensile Strength, Yield 1.03 - 2900 MPa
150 - 420000 psi
Average value: 576 MPa Grade Count:102
4.137 - 2571.74 MPa
<br>@Temperature -55.0 - 190 °C
600.0 - 373001 psi
<br>@Temperature -67.0 - 374 °F
Average value: 626 MPa Grade Count:17
Elongation at Break 0.000 - 50.0 %
0.000 - 50.0 %
Average value: 9.35 % Grade Count:33
2.40 - 6.90 %
<br>@Temperature 75.0 - 300 °C
2.40 - 6.90 %
<br>@Temperature 167 - 572 °F
Average value: 4.65 % Grade Count:1
Elongation at Yield 1.00 - 13.0 %
1.00 - 13.0 %
Average value: 3.49 % Grade Count:30
Modulus of Elasticity 0.00370 - 215 GPa
0.537 - 31200 ksi
Average value: 35.9 GPa Grade Count:99
1.572 - 164.095 GPa
<br>@Temperature -67.0 - 220 °C
228.0 - 23800.4 ksi
<br>@Temperature -88.6 - 428 °F
Average value: 57.7 GPa Grade Count:17
Flexural Yield Strength 92.0 - 1890 MPa
13300 - 274000 psi
Average value: 921 MPa Grade Count:33
108.937 - 1380.95 MPa
<br>@Temperature 50.0 - 177 °C
15800.0 - 200290 psi
<br>@Temperature 122 - 350 °F
Average value: 942 MPa Grade Count:7
Flexural Modulus 0.00350 - 205 GPa
0.508 - 29700 ksi
Average value: 56.0 GPa Grade Count:34
3.13711 - 109.075 GPa
<br>@Temperature 50.0 - 177 °C
455.007 - 15820.2 ksi
<br>@Temperature 122 - 350 °F
Average value: 63.0 GPa Grade Count:7
Compressive Yield Strength 2.76 - 1690 MPa
400 - 246000 psi
Average value: 358 MPa Grade Count:79
52.0 - 1585.79 MPa
<br>@Temperature -55.0 - 177 °C
7540 - 230000 psi
<br>@Temperature -67.0 - 351 °F
Average value: 574 MPa Grade Count:21
Compressive Modulus 0.0552 - 168 GPa
8.00 - 24300 ksi
Average value: 45.2 GPa Grade Count:59
12.0 - 162.027 GPa
<br>@Temperature -55.0 - 177 °C
1740 - 23500.4 ksi
<br>@Temperature -67.0 - 351 °F
Average value: 62.1 GPa Grade Count:16
Poissons Ratio 0.350 - 0.420
0.350 - 0.420
Average value: 0.389 Grade Count:10
Fracture Toughness 0.433 - 3.69 MPa-m½
0.394 - 3.36 ksi-in½
Average value: 1.33 MPa-m½ Grade Count:18
Shear Modulus 1.07 - 5.86 GPa
155 - 850 ksi
Average value: 3.20 GPa Grade Count:23
2.96475 - 35.0 GPa
<br>@Temperature 80.0 - 175 °C
430.007 - 5080 ksi
<br>@Temperature 176 - 347 °F
Average value: 13.7 GPa Grade Count:2
Shear Strength 6.76 - 137 MPa
980 - 19900 psi
Average value: 78.6 MPa Grade Count:51
11.0 - 164.095 MPa
<br>@Temperature -55.0 - 177 °C
1600 - 23800.0 psi
<br>@Temperature -67.0 - 351 °F
Average value: 58.8 MPa Grade Count:26
Adhesive Bond Strength 5.86 - 24.1 MPa
850 - 3500 psi
Average value: 12.8 MPa Grade Count:26
Toughness 51.0 - 541 J
37.6 - 399 ft-lb
Average value: 220 J Grade Count:8
Thermal Properties Metric English Comments
CTE, linear 16.0 - 85.5 µm/m-°C
8.89 - 47.5 µin/in-°F
Average value: 50.8 µm/m-°C Grade Count:37
98.0 - 180 µm/m-°C
<br>@Temperature >=27.0 °C
54.4 - 100 µin/in-°F
<br>@Temperature >=80.6 °F
Average value: 131 µm/m-°C Grade Count:9
Thermal Conductivity 0.140 - 1.28 W/m-K
0.972 - 8.88 BTU-in/hr-ft²-°F
Average value: 0.510 W/m-K Grade Count:28
Melting Point -80.0 - 130 °C
-112 - 266 °F
Average value: 40.0 °C Grade Count:4
Maximum Service Temperature, Air 25.0 - 260 °C
77.0 - 500 °F
Average value: 136 °C Grade Count:61
Softening Point 12.0 - 150 °C
53.6 - 302 °F
Average value: 74.4 °C Grade Count:33
Electrical Properties Metric English Comments
Electrical Resistivity 0.00100 - 8.10e+15 ohm-cm
0.00100 - 8.10e+15 ohm-cm
Average value: 2.07e+15 ohm-cm Grade Count:32
1.00e+7 - 1.50e+16 ohm-cm
<br>@Temperature 75.0 - 300 °C
1.00e+7 - 1.50e+16 ohm-cm
<br>@Temperature 167 - 572 °F
Average value: 3.36e+15 ohm-cm Grade Count:2
Dielectric Constant 2.96 - 5.40
2.96 - 5.40
Average value: 4.49 Grade Count:32
2.95 - 8.00
<br>@Temperature 70.0 - 150 °C
2.95 - 8.00
<br>@Temperature 158 - 302 °F
Average value: 5.49 Grade Count:3
2.95 - 8.00
<br>@Frequency 60.0 - 100000 Hz
2.95 - 8.00
<br>@Frequency 60.0 - 100000 Hz
Average value: 5.49 Grade Count:3
Dielectric Strength 14.4 - 51.2 kV/mm
365 - 1300 kV/in
Average value: 23.2 kV/mm Grade Count:38
Dissipation Factor 0.00600 - 0.500
0.00600 - 0.500
Average value: 0.335 Grade Count:3
0.00300 - 0.500
<br>@Temperature 149 - 150 °C
0.00300 - 0.500
<br>@Temperature 300 - 302 °F
Average value: 0.252 Grade Count:2
0.00300 - 0.500
<br>@Frequency 60.0 - 100 Hz
0.00300 - 0.500
<br>@Frequency 60.0 - 100 Hz
Average value: 0.252 Grade Count:2
Copyright © lookpolymers.com All Rights Reserved