Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm @Temperature 23.0 °C |
0.0010 - 0.0020 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® NY2115 Nylon 66 Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® PSU1700 Polysulfone General purpose polysulfone with excellent clarityAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ISO 2577 |
Polyram PlusTek RA303G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 50% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ISO 2577 |
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-1305/40 NAT PPS
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
Techmer Lehvoss Compounds Luvotech™ J-1305/40 BK5011 PPS
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |