Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | Across Flow; ISO 294-4 |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | Across Flow; ISO 294-4 |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | Across Flow; ISO 294-4 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (DAM) Information provided by Ravago |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 49 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | STN 64 0808 |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | 93°C; ASTM D955 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | 0.125 in, DAM; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all o the excellent properties of our general purpose acetal, has a volume .. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Aardvark Polymers AARTEL® 800 Rotational Molding Resin Aartel 800 is our high test, general purpose, acetal copolymer. Aartel 800 provides overall excellent performance for most applications and is available in natural (off white) and a wide range of st.. |
|||
Linear Mold Shrinkage | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
Kolon KOPA® KN333HFBL General Purpose Nylon 66 Middle viscosity, flexibleApplications Band cables for vehiclesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | RHODIA-EP |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | RHODIA-EP |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-60A/B Elastomer KE-1950-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Linear Mold Shrinkage | 0.019 - 0.025 cm/cm | 0.019 - 0.025 in/in | ASTM D955 |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | RHODIA-EP |
Solvay Technyl® A 205F Nylon 66, EH0 Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | RHODIA-EP |
Solvay Technyl® A 205F Nylon 66, EH50 Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Tipco Tipcolene® PPH-OIT - Unfilled Polypropylene Homopolymer Compound with Copper Inhibitor (Metal Deactivator) PP Homopolymer with Copper Inhibitor (Metal De-activator)Applications: Automotives & ElectricalProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO 294-4 |
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | |
Polyram RamTal PM340S4 Acetal, 20% Glass beads Reinforced 20% Glass beads reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.019 - 0.025 cm/cm | 0.019 - 0.025 in/in | |
Polyram RamTal PM1419 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM Data; MD |
BASF Ultraform N 2640 Z2 UNC Q600 POM Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM Data; MD |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM Data; MD |
BASF Ultraform W 2320 003 BK120 Q600 POM Ultraform W 2320 003 BK120 Q600 is a pigmented black, very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties .. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Ascend Performance Materials VYDYNE® 45 Nylon, Impact Modified, Weather Stable Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | Radial shrinkage of 10 cm o.d. sintered rod at 23°C |
Solvay Specialty Polymers Algoflon® 60BZ PTFE; Bronze Filled
(discontinued **) Data provided by the manufacturer.60 wt.% Bronze. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no .. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | |
Plastcom SLOVALEN PH 91 GF 10 PP, 10% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fibre. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased str.. |