Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Multibase Multi-Pro® 1012 C Polypropylene Calcium Carbonate Filler, 12% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE S906 Thermoplastic Elastomer, SBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE ZS2606 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.021 cm/cm | 0.014 - 0.021 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 S10 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 TF20 Nylon 6.6 for injection molding, 20% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ Nylon 6 Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1313
(discontinued **) PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
PolyOne Edgetek® NJ-000/000 Nylon 12
(discontinued **) Description/Features:General Purpose GradeHeat StabilizedHigh FlowUL 94 HBProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | |
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | Tool, Montell |
LyondellBasell Astryn BA16G Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade polypropylene copolymer, good flexibility, high impact strength, good colorability, good processability, good weath.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm @Thickness 1.59 mm |
0.014 in/in @Thickness 0.0625 in |
ASTM D955 |
Plastics Group Polifil® RMC-10 10% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Tipco Tipcolene® FPTC 30 HG - 30% Talc & Calcium Carbonate Polypropylene Homopolymer, High Gloss & Stiffness 30% Talc+Calcium Reinforced PP Homopolymer with High GlossApplications: Furniture & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
Polyram PlusTek PA100 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
Polyram PlusTek RA124 Nylon 6.6, Injection Molding Fast cycle polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Entec Hypro™ PP-HP12NS Homopolymer, 12 Melt Flow, Nucleated, Anti-stat, Injection Molding Homopolymer, 12 Melt Flow, Nucleated, Anti-stat, Injection MoldingInformation provided by Entec |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | |
E-Polymers TEKAMID® TB120L NCR , High Crystallinity PA6, DAM Precise injection, high crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
Linear Mold Shrinkage | 0.014 - 0.019 cm/cm | 0.014 - 0.019 in/in | ASTM D955 |
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L Calcium Reinforced |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Buckeye Polymers BP Flex D6707 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Ashley Polymers Ashlene® 827B Nylon 6 High impact, black, economy grade. Also available as: 827SB - Heat Stabilized, Black and 827SH - Heat Stabilized & UV Stabilized for Weatherability, Black.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Linear Mold Shrinkage | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | Injection |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid.. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm | 0.014 - 0.023 in/in | ASTM D955 |
Samyang Tribit® 1800 PBT, High Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800 is a high viscosity grade.Information .. |