Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0060 - 0.017 cm/cm | 0.0060 - 0.017 in/in | FRISETTA Test Method |
Nilit RECONYL B GV30 Recycled nylon 6 for injection molding, 30% glass fiber reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | LATI |
LATI LATILUB 88/50-20GRT K/10 PEEK Based, 10% Carbon Fiber Reinforced, 20% Graphite and PTFE Self Lubricating Plastic Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | With Flow; ISO 2577 |
Polykemi AB POLYabs N00 ABS Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.025 cm/cm | 0.0060 - 0.025 in/in | Average value: 0.0182 cm/cm Grade Count:13 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PPE 1462
(discontinued **) PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | Compression; ASTM D955 |
Plenco 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.014 cm/cm | 0.0060 - 0.014 in/in | ASTM D955 |
Kolon SPESIN® KP212G15V0BM G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, paintabilityApplications: A variety of cases and connectorsInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Global PC-1403 Standard Grade Polycarbonate Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Global PC-1410 General Purpose Polycarbonate Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Global PEI-110 Easy Flow, Polyetherimide Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D1299 |
Loxim 210 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | |
Momentive Performance Materials RTV11 White General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | MCI Method |
Mitsui APELâ„¢ APL6509T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | Isotropy |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | |
Styron CALIBRE™ 300 15 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.0080 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | GB/15585 |
Zhejiang Juner PC-A2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
Ecomass® 4703ZC87 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | |
E-Polymers SEPAZ® N5030 Nanoclay 4%, 30% Glass Fiber Reinforced Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
Beijing Chemical Industry KAIFA® 201-G30R PBT Resin 30% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | MD; ASTM D955 |
Aclo Accucomp ABS ABS804L High Impact Grade |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Asahi Kasei Thermylene® P-15FG-0860 15% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | GB/15585 |
Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |