Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0035 - 0.0045 cm/cm | 0.0035 - 0.0045 in/in | |
Ovation Polymers RIGITRON 20415 GF PBT, 15% Glass Reinforced PBT - Glass reinforced (15 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF10030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | Post shrinkage is 0.17% at 72hr 120°C.; ASTM D955 |
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for .. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
SK Chemicals SKYTHANE® R185A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D6289 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PA301G7 Nylon 6.6, Heat Stabilized 35% Glass Fiber Heat stabilized 35% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB300G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | Injection Molding; ISO 2577 |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB305G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized and UV stabilized polyamide 6 approved and listed by W.R.C and NSF/ANSI 61 international for potable waterInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB306G6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
Polyram PlusTek PB310G6 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AR-37 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell BT-37 Nylon 6, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | restricted |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AR-17 Nylon 66, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell AT-17 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | ASTM D955 |
Adell BJ-17 Nylon 6, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0035 - 0.0040 cm/cm | 0.0035 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® AM-10CF-20GF/000 HS Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0035 cm/cm | 0.0035 in/in | LATI |
LATI LARAMID G/35 35% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |