Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 60
60
ASTM D785
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Ultimate 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 5.90 GPa
856 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Gardner Impact 0.300 J
0.221 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Flammability, UL94 HB
HB