Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Loose |
Nyco NYAD® 400 Wollastonite Chemically treated powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an .. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.950 g/cc | 0.0253 - 0.0343 lb/in³ | |
Magyar Aluminum ALO-P54 Alumina Alumina for Polishing |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Lucite International Colacryl ® CRG107 Specialty Acrylic Resin Colacryl® CRG107 is a hard, methyl methacrylate based, acrylic resin with exceptional pigment wetting properties. It is soluble in chlorinated hydrocarbons, ketones and lower esters and compatibl.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Scott Density; ASTM B329 |
H.C. Starck FeCoCu Prealloyed Metal Powder A new prealloyed metallic powder of high sinter-activity with ideally homogenized constituents at an atomic level. The primary particles of very fine grain size are loosely agglomerated to agglomera.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 60 |
Lanxess Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Solvay JAGUAR® C 14 S Surfactant Description: Substantive to hair and skin. Provides excellent wet combing and soft non-tacky feel to hair.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name : GUAR HYDROXYPROPYLTRIMONIUM CHLOR.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Solvay JAGUAR® C 17 Surfactant Description: Highly substantive to hair and skin. Recommended for high conditioning shampoos and moisturizing body washes. Enhances deposition of actives such as silicone, anti-dandruff agents and m.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Solvay RHODICARE T Surfactant Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydrat.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Powder Density; ISO 60 |
Vyncolit 4523 XB Novolac Phenolic Organic and inorganic filled phenolic molding compound with good mechanical and thermal properties. Improved heat resistance compared to organic filled compounds.USES: Fuse holders, brush holders, .. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Powder Density; ISO 60 |
Vyncolit X689 Novolac Phenolic Glass fiber filled and molybdeendisulfide modified phenolic molding compound with excellent mechanical and thermal properties and lower thermal expansion coefficient. It has excellent friction prop.. |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | Powder Density; ISO 60 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Bulk Density | >= 0.700 g/cc | >= 0.0253 lb/in³ | |
Chosun Refractories B-1 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
Chosun Refractories CFA-2 Ceramic Foam Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | |
BASF Ultramid® A27 E PA66 Description: Ultramid® A27 E is a polyamide 66 grade for compounding.Information provided by BASF |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Bulk Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM D1895 |
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |