Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Loose |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Zircar Zirconia HfF-100 Hafnia Felt Insulation Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D4895 |
3M Dyneon™ TF 2072 PTFE
(discontinued **) Processable by standard paste extrusion methodTF 2071 and TF 2072 have a wide processing range because of high maximum allowable reduction ratioTF 2072 is recommended for thin-wall, small diameter t.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
Magyar Aluminum ALO-DF2 Alumina Alumina for Polishing |
|||
Bulk Density | 0.500 - 0.580 g/cc | 0.0181 - 0.0210 lb/in³ | ASTM D1895 |
LG Chemical LS100 PVC General Description: LS100 is a general-purpose product used for soft and hard products and is most widely used in PVC grade.Main Applications: Pipe, power cable jacket, leather, sheets, hoses, soft.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Tap Density |
Momentive Performance Materials AC6103 Boron Nitride (BN) Powder Agglomerate of hexagonal BN crystals. AC6103 powders are granular with good flow and blend characteristics as well as high thermal conductivity and good lubrication qualities. Information provided.. |
|||
Bulk Density | 0.500 - 0.900 g/cc | 0.0181 - 0.0325 lb/in³ | |
Solvay Chemicals NOCOLOK® CB Flux Potassium Silicofluoride Reactive flux for brazing of aluminumCAS-No.: 16871-90-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided .. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
Shandong Dongyue Polymer DF-21 PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Solvay SOPROPHOR® K/202 Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ABSORBED SURFACTANTSolubility: Dispersible in water. Insoluble in polar and aromatic solvents.Available in: Asia Pacific.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Size E (apparent) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Size E (apparent) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | >= 0.500 g/cc | >= 0.0181 lb/in³ | |
Chosun Refractories A-2 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® FR 495 PP copolymer based flame-retardant compound Fields of application: Injection moulded, or moulded articles (> 1,5 mm thickness) produced via Direct LFT processesExamples: Moulding parts such a under body panels, door modules, industrial parts,.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
ALM PA 250 Nylon 12 SLS Prototyping Polymer Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® 1C PA6/66 (Dry) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Asahi Glass Fluon® CD141 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
BASF Sicopal® Brown K 2795 Color Additive Chemical Structure: Fe/Cr-oxideApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA PETP, CA/CAB and UPRecommendations for food applications: .. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® Seal-Fit PA6/66 (Dry) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ISO 60 |
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |