Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.020 - 0.0219 cm/cm @Time 86400 sec |
0.020 - 0.0219 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Time 86400 sec |
0.020 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.0219 cm/cm @Time 86400 sec |
0.020 - 0.0219 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Time 86400 sec |
0.020 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.025 cm/cm @Time 86400 sec |
0.020 - 0.025 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.025 cm/cm @Time 86400 sec |
0.020 - 0.025 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific) LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific) LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66 LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas .. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.030 cm/cm @Time 86400 sec |
0.020 - 0.030 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific) LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Time 86400 sec |
0.020 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 cm/cm @Temperature 240 °C |
0.020 in/in @Temperature 464 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |