Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.020 - 0.0219 cm/cm

@Time 86400 sec
0.020 - 0.0219 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer
LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 - 0.022 cm/cm

@Time 86400 sec
0.020 - 0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer
LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 - 0.0219 cm/cm

@Time 86400 sec
0.020 - 0.0219 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer
LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 - 0.022 cm/cm

@Time 86400 sec
0.020 - 0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer
LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 - 0.025 cm/cm

@Time 86400 sec
0.020 - 0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
Linear Mold Shrinkage, Transverse 0.020 - 0.025 cm/cm

@Time 86400 sec
0.020 - 0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F..
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66
LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66
LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific)
LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66
LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER
LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE
LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas ..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.030 cm/cm

@Time 86400 sec
0.020 - 0.030 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly
LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66
LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-loy W3000 PBT
LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ..
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Temperature 240 °C
0.020 in/in

@Temperature 464 °F
ASTM D3392
DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Copyright © lookpolymers.com All Rights Reserved