Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Water Absorption 5.7 %
5.7 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 1.7 %
1.7 %
Humidity Absorption; Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
ISO 527-1/-2
Elongation at Break 5.2 %
5.2 %
ISO 527-1/-2
Tensile Modulus 11.0 GPa
1600 ksi
ISO 527-1/-2
Charpy Impact Unnotched 10.5 J/cm²

@Temperature 23.0 °C
50.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
11.5 J/cm²

@Temperature -30.0 °C
54.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
IEC 60250
3.5

@Frequency 100 Hz
3.5

@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1
Dissipation Factor 0.0090

@Frequency 100 Hz
0.0090

@Frequency 100 Hz
IEC 60250
0.015

@Frequency 1e+6 Hz
0.015

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
High impact or impact modified Yes
Injection molding Yes
Release Agent Yes
With Fillers Yes
Users viewing this material also viewed the following: