Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.34 - 1.85 g/cc | 0.0484 - 0.0668 lb/in³ | Average value: 1.58 g/cc Grade Count:24 |
Overview of materials for Polyarylamide, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values.. |
|||
Density | 0.549 - 1.85 g/cc | 0.0198 - 0.0668 lb/in³ | Average value: 1.37 g/cc Grade Count:538 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Density | 1.46 - 1.85 g/cc | 0.0527 - 0.0668 lb/in³ | Average value: 1.55 g/cc Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Density | 1.25 - 1.85 g/cc | 0.0452 - 0.0668 lb/in³ | Average value: 1.53 g/cc Grade Count:4 |
Overview of materials for Phenolic, Ablative Coating This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Ablative Coating". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 1.04 - 1.85 g/cc | 0.0376 - 0.0668 lb/in³ | Average value: 1.31 g/cc Grade Count:378 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.60 - 1.85 g/cc | 0.0578 - 0.0668 lb/in³ | Average value: 1.70 g/cc Grade Count:62 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Density | 1.81 - 1.85 g/cc | 0.0654 - 0.0668 lb/in³ | ISO R 1183 |
Fainplast Compounds CRKA 78 Flexible PVC, Flame Retardant Electrical Bedding Lead Free Flame retardant bedding |
|||
Density | 1.80 - 1.85 g/cc | 0.0650 - 0.0668 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom.. |
|||
Density | 1.79 - 1.85 g/cc | 0.0647 - 0.0668 lb/in³ | Molded |
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic.. |
|||
Density | 1.65 - 1.85 g/cc | 0.0596 - 0.0668 lb/in³ | Molded |
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by.. |
|||
Density | 1.35 - 1.85 g/cc | 0.0488 - 0.0668 lb/in³ | Average value: 1.48 g/cc Grade Count:108 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.81 - 1.85 g/cc | 0.0654 - 0.0668 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 83/M Flexible PVC, Extrusion Covering copper pipes |
|||
Density | 1.75 - 1.85 g/cc | 0.0632 - 0.0668 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1200H-24 Polyester SMC
(discontinued **) Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni.. |
|||
Density | 1.75 - 1.85 g/cc | 0.0632 - 0.0668 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |
|||
Density | 1.75 - 1.85 g/cc | 0.0632 - 0.0668 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |