Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 - 1.20 g/cc | 0.0426 - 0.0434 lb/in³ | ASTM D792 |
Plaskolite Optix® CA-81 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Cast 100 3D Printing Polymer High reactivity and low viscosity. Excellent dimensional stability.Fulfills the high demands place on digital process chain.Information provided by Genistar. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Clear 100 3D Printing Polymer Ultra clear.Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Wide range of medical applicationInformation provided by G.. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Model 100 3D Printing Polymer Allows production of precise components; high workability.Used for dental applications from models for restorations to orthodontics.Information provided by Genistar. |
|||
Density | 1.02 - 1.20 g/cc | 0.0368 - 0.0434 lb/in³ | Average value: 1.05 g/cc Grade Count:101 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Density | 0.700 - 1.20 g/cc | 0.0253 - 0.0434 lb/in³ | Average value: 1.17 g/cc Grade Count:249 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Hybrid Plastics NanoBondâ„¢ UV Curable Adhesive Generally used for dental and optical applications.Information provided by Hybrid Plastics |
|||
Density | 1.13 - 1.20 g/cc | 0.0408 - 0.0434 lb/in³ | 265 Resin |
Lord Adhesives Versilok® 265 / 254 Acrylic Adhesive LORD Versilok® 265/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Density | 1.12 - 1.20 g/cc | 0.0405 - 0.0434 lb/in³ | Wet Density (Depending on Tamp Density) |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® T22 Tamping Mix Description: THERMOSEAL® T22 FIBERPAK® TAMPING MIX is a wet taping mix made up of bulk refractory fibers and a high temperature binder system. T22 FIBERPAK® TAMPING MIX is particularly good.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A7711 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8510 TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8521 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8521H TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1184 |
Fainplast Compounds GS 54/AM Flexible PVC, Electrical Plugs Lead Free Plugs anti mould |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 59/F Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 59/T Flexible PVC, Injection Molding for Footwear Crystal sandals |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 60/AS Flexible PVC, Injection Molding for Footwear Oil resistent and antistatic soles |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 75/R1 Flexible PVC, Injection Molding for Footwear Soles antiaccident shoes |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 50 Flexible PVC, Extrusion Modified with Rubber Hydrocarbon and diesel oil resisting sheath |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 55/A Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 55 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 61/K1-AM Flexible PVC, Transparent Extrusion Transparent profiles embossed anti mould |
|||
Density | 1.15 - 1.20 g/cc | 0.0415 - 0.0434 lb/in³ | |
BecauseWeCare BF90 Biodegradable Plastic Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the vari.. |
|||
Density | 1.14 - 1.20 g/cc | 0.0412 - 0.0434 lb/in³ | Average value: 1.17 g/cc Grade Count:6 |
Overview of materials for Silicone Polyurethane, Polycarbonate Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.15 - 1.20 g/cc | 0.0415 - 0.0434 lb/in³ | Average value: 1.18 g/cc Grade Count:14 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 0.920 - 1.20 g/cc | 0.0332 - 0.0434 lb/in³ | Average value: 0.987 g/cc Grade Count:123 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Density | 1.10 - 1.20 g/cc @Temperature 285 - 285 °C |
0.0397 - 0.0434 lb/in³ @Temperature 545 - 545 °F |
Average value: 1.19 g/cc Grade Count:27 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Density | 0.970 - 1.20 g/cc | 0.0350 - 0.0434 lb/in³ | Average value: 1.12 g/cc Grade Count:8 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |