Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.970 g/cc | 0.0350 lb/in³ | ASTM D792 |
Network Polymers NPP 25-1503 G10 Description: Glass Reinforced PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | TA4820A |
Permabond TA4820 Structural Acrylic Adhesive PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | TPE-0105 (ASTM D792) |
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Density | 0.969 g/cc | 0.0350 lb/in³ | ASTM D792 |
PolyOne Maxxam® FR PE 113 Low Density Polyethylene (LDPE)
(discontinued **) Applications:Wire and cable insulationInformation provided by PolyOne Corporation. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | Melt |
Covestro Apec® 2000 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | Melt |
Covestro Apec® DP 1-9379 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ha.. |
|||
Density | 0.970 g/cc @Temperature 23.0 °C |
0.0350 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Inno-Comp INNOPOL® CS 2-4210 10% Chalk-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-4210 is a 10% chalk-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-4210 is developed for producin.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 1183 |
Lucobit Lucobit® 1210 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | |
Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 29°C. Average solids: 48%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, and bare copper coils... |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ASTM D792 |
Washington Penn Medium Impact Copolymer 10% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 1183 |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | Melt |
Covestro Desmopan® DP 9095AU Polyurethane injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood wear resistancelow warpargeshort cycle timesApplicationEar-tagsPreprocessingMax. Water content |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 1183/A |
ExxonMobil Exxtral™ BMU130P Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ CMU 101 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance and good UV resistance are required.Availa.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ASTM D792 |
DuPont™ Surlyn® 8150 Ionomer Resin, Sodium Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and .. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ASTM D792 |
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 700 Coating Information provided by Dow Corning |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | DIN 53479 |
Dynasol Solprene® 303 Random-Block Copolymer Solprene 303 is a linear random-block styrene-butadiene copolymer with 46% styrene content, 11% present as a polystyrene block. S-303 is used in vulcanized microcellular shoe soles, it provides hard.. |
|||
Density | 0.969 g/cc | 0.0350 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0334T10L1 Talc Reinforced |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | |
BASF 1,2-Pentanediol Formula: C5H12O2CAS: 5343-92-0Description: 1,2-Pentanediol is a colorless to yellowish liquid, with a pungent odor. It is miscible with water.Synonyms: Pentane-1,2-diolApplications: Intermediate us.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 2781 |
Alliance Polymers Viprene™ G50A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 2781 |
Alliance Polymers Viprene™ G60A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G60A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 2781 |
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 2781 |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ASTM D792 |
Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled Increased flex w/ living hinge propertiesCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be cus.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 2781 |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Density | 0.970 g/cc | 0.0350 lb/in³ | TPE-0105 (ASTM D792) |
Advanced Elastomer Systems Santoprene® 281-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |