Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.14 - 1.20 g/cc
0.0412 - 0.0434 lb/in³
Average value: 1.17 g/cc Grade Count:6
Melt Flow 17.0 - 52.0 g/10 min
17.0 - 52.0 g/10 min
Average value: 28.5 g/10 min Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Shore A 80.0 - 90.0
80.0 - 90.0
Average value: 88.0 Grade Count:5
Tensile Strength, Ultimate 29.6 - 54.2 MPa
4290 - 7850 psi
Average value: 40.2 MPa Grade Count:6
Tensile Strength, Yield 4.85 - 37.9 MPa
704 - 5490 psi
Average value: 14.8 MPa Grade Count:6
Elongation at Break 344 - 530 %
344 - 530 %
Average value: 438 % Grade Count:6
Flexural Modulus 0.0395 - 0.0414 GPa
5.73 - 6.00 ksi
Average value: 0.0405 GPa Grade Count:3
Tear Strength 82.4 - 94.7 kN/m
470 - 540 pli
Average value: 88.2 kN/m Grade Count:3
Taber Abrasion, mg/1000 Cycles 20.0 - 144
20.0 - 144
Average value: 73.7 Grade Count:3
Compression Set 15.0 - 33.0 %
15.0 - 33.0 %
Average value: 24.7 % Grade Count:3
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -7.00 - 5.00 °C
19.4 - 41.0 °F
Average value: -2.00 °C Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 185 - 210 °C
365 - 410 °F
Average value: 198 °C Grade Count:6