| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
|
Multibase Multi-Flex® TPE A 7606 GRAPHITE
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | |
|
Premix Thermoplastics PREADD AS 133
PREADD AS 133 is a polyethylene based antistatic masterbatch developed for polyolefines. The active additive in PREADD AS 133 is an amide giving a good antistatic effect already at low dosing levels..
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D792 |
|
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin
Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical ..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend
The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring ..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
|
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
(discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | Exxon Method |
|
ExxonMobil Escorene® LL-5002 LLDPE Compounding Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. LL-5002 also exhibits good toughness and envi..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
M. Holland Company LL102 LLDPE
(discontinued **)
Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c)..
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
Eastman 1550A Polyethylene
(discontinued **)
Injection molding gradeUnless otherwise noted, all tests are run at 23°C and 50% RH. Where required, samples are compression molded per ASTM D1928.Information from manufacturer data sheet.Eastman ..
|
|||
| Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D792 |
|
NOVA Chemicals Novapol® LM-1019-A LDPE Masterbatch Resin
(discontinued **)
Features: easy processing, good dispersion.Applications: masterbatch/compounding.Data provided by the manufacturer.
|
|||
| Density | 0.919 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
|
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **)
LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D 792 |
|
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin
PF-0218-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur..
|
|||
| Density | 0.919 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | |
|
Kazanorgsintez 15313-003 High Pressure Polyethylene
Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac..
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent ..
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
LyondellBasell Petrothene® GA616050 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 616-050 is a linear low density polyethylene resin which can be dry blended with low density polyethylene coating resins to produce linear low extrusion coatings. LDPE grad..
|
|||
| Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
LyondellBasell Petrothene® NA951000 Low Density Polyethylene
ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1872/1 |
|
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film
Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l...
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
UBE F120N Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
UBE R300 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
Westlake EN1817AA Low Density Polyethylene
Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli..
|
|||
| Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE
Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng..
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | Base Density; ASTM D1505 |
|
Chevron Phillips Marlex® M151 LLDPE Pipe and Corrugated Extrusion Resin
Characteristics: Good long-term hoop strengthExtended outdoor lifeClean N550 carbon blackApplications: PipesNot recommended for contact with food productsInformation provided by Chevron Phillips.
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM-D792 |
|
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer
X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled..
|
|||
| Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM-D792 |
|
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer
FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this pr..
|
|||
| Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM-D1505 |
|
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer
LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processin..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM-D792 |
|
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve..
|
|||
| Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
|
ExxonMobil Exceed™ 1018 EA Blown Film Resin
(discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
|
|||
| Density | 0.919 - 0.930 g/cc | 0.0332 - 0.0336 lb/in³ | Average value: 0.922 g/cc Grade Count:5 |
|
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
|
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
|
|||
| Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D4883 |
|
Westlake Hifor SC74560-F Clear Polyethylene
(discontinued **)
Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc..
|
|||
| Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
|
Amco PRIMATOP LLDPE 009919B Linear Low Density Polyethylene, Butene Copolymer for Film
LLDPE 009919B features excellent toughness and strength when drawn down to thin gauges. Applications include blending resin, industrial packaging, coextrusion, industrial liners, and garment bags.Fo..
|
|||