Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO.1183 DIN.53479 |
Omnia Plastica PPS GF40 Polyphenylenesulphide Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. .. |
|||
Density | 1.64 - 1.84 g/cc | 0.0592 - 0.0665 lb/in³ | Average value: 1.71 g/cc Grade Count:30 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Density | 1.64 - 2.10 g/cc | 0.0592 - 0.0759 lb/in³ | Average value: 1.85 g/cc Grade Count:35 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
LATI Latiohm 80-04 PD01 G/30 PPS, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyphenylene Sulfide (PPS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RX01075 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX01075 is a compound based on Nylon 66 resin containing PTFE, Mineral. Added features of this material include: Heat Stabilized. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA 12 (Asia Pacific) LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP SFL2A PA12 LNP* LUBRICOMP* SFL2A is a compound based on Nylon 12 resin containing 50% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East) VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Stir SpA E 2055 (PVC) Application: Extrusion tubular gasketInformation provided by STIR SpA |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT LNP THERMOCOMP* WF008 is a compound based on PBT resin containing 40% Glass Fiber. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Unitika A1025GO PA6, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
Polyplastics Duranex® HN7330 Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH |
3M AC-236 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH |
3M AC-236 Class C-80 Aerospace Sealant 3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance .. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
A. Schulman ComAlloy Hiloy® 714 PPS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.64 g/cc @Temperature 23.0 °C |
0.0592 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | |
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | cured 14 days @ 50% RH |
3M AC-236 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 |
Plenco 50335 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |