Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Ixef®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Heat Stabilized; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High StiffnessUses: Appliance Components; Appliances; Automotive Applications; Business Equipment; Furniture; Gears; Industrial Applications; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other ToolsInjection Molding Notes: Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding.Additional Properties: Moisture Absorption - Internal Method 1.5 %Automotive Specifications GM GM7001M PAMXD6(A4,A22,A42,A64,BA651,G30,MS1650,NS335) Color: 9000 BlackInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.64 g/cc
0.0592 lb/in³
ISO 1183
Filler Content 50 %
50 %
Glass Fiber
Water Absorption 0.16 %

@Time 86400 sec
0.16 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 235 MPa
34100 psi
ISO 527-2
Elongation at Break 1.8 %
1.8 %
ISO 527-2
Tensile Modulus 20.0 GPa
2900 ksi
ISO 527-2
Flexural Strength 360 MPa
52200 psi
ISO 178
Flexural Modulus 18.5 GPa
2680 ksi
ISO 178
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.20 J/cm
13.5 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
9.44 µin/in-°F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Annealed; ISO 75-2/A
Flammability, UL94 HB
HB
Oxygen Index 25 %
25 %
ISO 4589-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IIEC 60093
Dielectric Constant 4.6

@Frequency 1.10e+8 Hz
4.6

@Frequency 1.10e+8 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
711 kV/in
IEC 60243-1
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 260 °C
482 - 500 °F
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Melt Temperature 280 °C
536 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 120 °C

@Time 1800 - 5400 sec
248 °F

@Time 0.500 - 1.50 hour
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant