Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D223 GF10 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Density | 1.55 - 1.99 g/cc | 0.0560 - 0.0719 lb/in³ | Average value: 1.64 g/cc Grade Count:63 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications... |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA (Asia Pacific) LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | Dry; ISO 1183 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM F1315 |
Thermoseal KLINGERSIL® C-4430 Compressed Inorganic Fiber Gasketing Synthetic FiberNitrile BinderExcellent Steam SheetExcellent Chemical ResistanceGood Creep RelaxationGeneral Purpose SheetInformation provided by Thermoseal Inc. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Polyplastics Duranex® CN7015 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
CPC - Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet Flametec™ CPVC made from Corzan® 4910 white 120 compound is a high heat, corrosion resistant chlorinated polyvinyl chloride sheet. Because of its excellent corrosion resistance at elevated tempera.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
BASF Petra® 7030 GY6128 30% Glass Filled PET Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It o.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 551GT20S PBT Resin Glass fiber and mineral filled, flame retardant, low warpage, superior electrical performance, surface glossInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Addiplast Addinyl A2H V25 Flame Retardant Nylon 66, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast. |
|||
Density | 1.55 g/cc @Temperature 25.0 °C |
0.0560 lb/in³ @Temperature 77.0 °F |
Liquid |
Asahi Glass ASAHIKLIN AK-225DH Hydrochlorofluorocarbon Solvent AK-225DH was developed as a solvent dewatering and drying system to remove water from the surface of various parts and assemblies. AK-225DH is a mixture of AK-225 and a drying agent to give it rapid.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 301-G30F PBT Resin 30% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DSM Arnite® TV4 261 KL PBT-GF30 30% Glass Reinforced, Light Stabilized |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® MN301-G35 Nylon 66 Resin 35% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
LATI Latiohm 75/4-03 PD01 G/20 PBT, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
LATI Latiohm 75/4-08 PD01 G/30 PBT, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |