| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled , Nylon 66, Glass Fiber Filled, Flame Retardant |
| Manufacturer | Addiplast |
| Trade Name | Addinyl |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Addiplast Addinyl A2H V25 Flame Retardant Nylon 66, 25% Glass Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 89 | 89 | Conditioned; ISO 868 |
| 90 | 90 | ISO 868 | |
| Tensile Strength at Break | 110 MPa | 16000 psi | Conditioned; ISO R 527 |
| 140 MPa | 20300 psi | ISO R 527 | |
| Elongation at Break | 5.0 % | 5.0 % | ISO R 527 |
| 5.0 % | 5.0 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 6.50 GPa | 943 ksi | Conditioned; ISO 178 |
| 8.50 GPa | 1230 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 9.50 kJ/m² | 4.52 ft-lb/in² | ISO 180/1A |
| 10.5 kJ/m² | 5.00 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/IeU |
| 6.00 J/cm² | 28.6 ft-lb/in² | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/IeA |
| 1.10 J/cm² | 5.23 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F | ISO 75-2/AF |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
| Oxygen Index | 34 % | 34 % | ISO 4589 |
| Glow Wire Test | 960 °C | 1760 °F | CEI 60695/2/1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Conditioned; CEI 60093 |
| 1.00e+14 ohm | 1.00e+14 ohm | CEI 60093 | |
| Comparative Tracking Index | 275 V | 275 V | CEI 60112/Solution A |