Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature range, low moisture absorption, excellent chemical resistance and excellent electrical properties.Features: Fast Molding Cycle; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Low Moisture Absorption; LubricatedUses: Abrasive Cleaning Material; Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Thick-walled Parts; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D6779 PA102G45; TYCO 100-1632 Color: BK-324 BlackInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
Dry; ISO 1183
Filler Content 45 %
45 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Dry
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 186 MPa
27000 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 15.2 GPa
2200 ksi
ASTM D638
Flexural Yield Strength 269 MPa
39000 psi
ASTM D790
Flexural Modulus 13.1 GPa
1900 ksi
ASTM D790
Compressive Strength 159 MPa
23100 psi
ASTM D695
Shear Strength 75.8 MPa
11000 psi
ASTM D732
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 320 °C
608 °F
Dry; ISO 11357-3
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
ASTM D257
Dielectric Constant 4.0

@Frequency 1.00e+6 Hz
4.0

@Frequency 1.00e+6 Hz
ASTM D150
4.9

@Frequency 60.0 Hz
4.9

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm

@Thickness 1.59 mm
635 kV/in

@Thickness 0.0626 in
ASTM D149
Dissipation Factor 0.024

@Frequency 60.0 Hz
0.024

@Frequency 60.0 Hz
ASTM D150
0.037

@Frequency 1.00e+6 Hz
0.037

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
UL 746
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Processing Properties Metric English Comments
Processing Temperature 79.4 °C
175 °F
Hopper
Rear Barrel Temperature 318 - 324 °C
604 - 615 °F
Front Barrel Temperature 327 - 332 °C
621 - 630 °F
Melt Temperature 329 - 343 °C
624 - 649 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Lubricant
Mold Release
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved