Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 SG-GV 2515 Nylon 6 for injection molding, 25% mineral filled and 15% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ±0.03 g/cm³; DIN 53479 |
PolyOne Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183/A |
Grupo Repol Dinalon® B1S25 M404 PA6 40% Mineral Charge Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Lanxess Pocan® KU 1-7635 POS151 000000 PBT + PC, 30% Glass Fiber PBT+PC, 30% glass fibers, injection molding, low tendency to warp, improved surface finish, UV-stabilized |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer LNP LUBRICOMP* KL004 is a compound based on Acetal Copolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific) LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF43 L BKN001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackProcessing Method: Injection M.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO 0150 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 15% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PC/PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 (Asia Pacific) LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabil.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | Relative Density; ISO 1183 |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183-87 |
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183-87 |
Wellman Wellamid® MRGF25/15 42H-BK167A Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced GM 167A Black color matchAll information provided by Wellman Engineered Resins. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
3M Novec™ 1720 Electronic Grade Coating 3M™ Novec™ 1720 Electronic Grade Coating adds easy clean capabilities to surfaces such as glass flat panel displays and mobile electronic device components. It is a clear, 0.1 wt% fluorosilane pol.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | |
A. Schulman ComAlloy Comtuf® 615 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 76/E Flexible PVC, Sheathing General purposes |