Material Notes:
3M™ Novec™ 1720 Electronic Grade Coating adds easy clean capabilities to surfaces such as glass flat panel displays and mobile electronic device components. It is a clear, 0.1 wt% fluorosilane polymer in a hydrofluoroether solvent.Features and Benefits:Easy application and processing - air dries in seconds and should be thermally cured for best performanceAdheres to a variety of surfaces including glass, metals and metal oxidesProvides excellent anti-wetting, anti-stiction and anti-migration propertiesContains no volatile organic compounds (VOCs) and has low global warming potentialIs optically transparent and contributes no additional haze and no loss of clarityInformation provided by 3M
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Solids Content 0.10 %
0.10 %
fluoropolymer
Thermal Properties Metric English Comments
Boiling Point 61.0 °C
142 °F
of Solvent
Glass Transition Temp, Tg -110 °C
-166 °F
Optical Properties Metric English Comments
Refractive Index 1.34
1.34