Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.30 g/cc | 0.0470 lb/in³ | DIN 53479 |
Qualchem Danamid AFGF-20 Polyamide 66, 20% Glass Fiber Reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
Victrex® PEEK 150UF10 Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliant.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
Lanxess Pocan® B 1305 000000 PBT PBT, non-reinforced, injection molding |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
Lanxess Pocan® DP 1105 000000 PBT PBT, non-reinforced, injection molding, extrusion, improved flowability |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ajedium™ KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PC CF20 FR IM BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Frame Retardant, Impact Modified and Semi Conductive.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Density | 1.30 g/cc @Temperature 25.0 °C |
0.0470 lb/in³ @Temperature 77.0 °F |
Liquid |
Shandong Dongyue Shenzhou New Material Co Hexafluoropropene Oxide (HFPO) Conformable with: Q/DYS 002-2007Hexafluoropropene Oxide (HFPO) is a kind of colorless and uninflammable gas. It is easy to be liquefied under pressure, and generally be used as special intermediate.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF20 L BK001 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 8376102Information provid.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific) LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 LNP* THERMOCOMP* RF0079SZ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN®-N ASG30 SAN resin Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Chase Plastics CP Pryme® N320L (Dry) Nylon 6, 20% Glass Fiber Reinforced, Lubricated, Recycled Content Features: LubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183-1 |
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Density | 1.30 g/cc @Thickness >=0.000 mm |
0.0470 lb/in³ @Thickness >=0.000 in |
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3 |
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Reinforced with finer fabric than Etronax MF. Can be used, in particular, for mechanical applications where fine tolerances and smoother surface finish are requ.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® S600F10 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 BK851 is an unreinforced lubricated medium high viscosity black polybutylene tere.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | D792 |
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Density | 1.30 - 1.31 g/cc | 0.0470 - 0.0473 lb/in³ | ISO 1183 |
Beijing Ranger Chem BLUESTAR® 1079 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |