Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792-91 |
Multibase Multi-Pro® 4005 M I Medium Impact 40% Filler Content Polypropylene Multi-Pro 4005 M I is a chemically coupled reinforced polypropylene compound featuring high flex modulus and high impact under retention of the heat resistance properties. The product is designed f.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 4010 M Polypropylene Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | STN 64 0111 |
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
Polyplastic Armlen® PP MF 40-3M Polypropylene Copolymer, 40% Calcium Carbonate Injection moldingInformation provided by PolyPlastic Group. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D241 PBT, Impact Modified Information provided by Polykemi AB |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**) Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | |
Polimeri Europa KOBLEND PCA PD 935 G4 PC+ABS, 20% Glass Fiber
(discontinued **) Symbol according to ISO 1043/1/2: PC+ABS (GF) Injection moulding grade, reinforced with 20% glass fibres, high stiffness, very good dimensional stability. Main application fields: structural non a.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP ICL34 PA6.12 LNP* LUBRICOMP* ICL34 is a compound based on Nylon 6/12 containing 20% Carbon Fiber, 15% PTFE. Added features include: Wear Resistant. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Techmer ES HiFill® HIPS GF30 30% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07435 LNP* THERMOCOMP* is a compound based on Miscellaneous resin containing Proprietary Filler(s). Added feature of this grade is: Plateable. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF003AXH PA 66 LNP* THERMOCOMP* RF003AXH is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | |
Goodfellow Polyaramid/Polyphenylene Sulfide Composite Sheet or Rod 25% Polyaramid fiber - PPS Matrix. Information provided by Goodfellow. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
DSM Stanyl® TW371 (DAM) Nylon 46 Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 001/AL Flexible PVC, Insulation Lead Free General purposes suitable for food contact according to CEE 90/128 |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black Information provided by Eurotec® |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness Data provided by Adell Plastics, Inc. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | |
Arlon CP-434R Bulk Compound Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | |
3M EPS-400 Heat Shrink Tubing 3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 1410B Polycarbonate, 8-10% Glass Reinforced A rigid black polycarbonate, for applications requiring superior dimensional stability and overall toughness. Contains 8-10% glass reinforcement. Also available: 1413B, UV stabilized.Data provided.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 1513 Polycarbonate A rigid flame retardant polycarbonate, UV stabilized in black for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183/A |
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |