Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.06 - 1.43 g/cc | 0.0383 - 0.0517 lb/in³ | Average value: 1.10 g/cc Grade Count:49 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.11 - 1.43 g/cc | 0.0401 - 0.0517 lb/in³ | Average value: 1.21 g/cc Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.43 - 1.43 g/cc @Temperature 215 - 215 °C |
0.0517 - 0.0517 lb/in³ @Temperature 419 - 419 °F |
Average value: 1.43 g/cc Grade Count:1 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.02 - 1.43 g/cc | 0.0368 - 0.0517 lb/in³ | Average value: 1.20 g/cc Grade Count:86 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.21 - 1.43 g/cc | 0.0437 - 0.0517 lb/in³ | Average value: 1.30 g/cc Grade Count:10 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.36 - 1.43 g/cc | 0.0491 - 0.0517 lb/in³ | Average value: 1.40 g/cc Grade Count:31 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.10 - 1.43 g/cc | 0.0397 - 0.0517 lb/in³ | Average value: 1.21 g/cc Grade Count:40 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 310/K1 Rigid PVC, Antishock Extrusion Lead Free Mat effect antishock profiles |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® FA C063 EEA High performance Crimped staple oxidized textile fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® FA C063 SSC High performance Crimped staple oxidized textile fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® FA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not b.. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® SA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not b.. |
|||
Density | 1.41 - 1.43 g/cc | 0.0509 - 0.0517 lb/in³ | |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Density | 1.41 - 1.43 g/cc | 0.0509 - 0.0517 lb/in³ | Dry Density |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) at 50% RH Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction prope.. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 83/1 Flexible PVC, Sheathing Sheath coaxial TV Cable |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1186 |
Fainplast Compounds GK 72/R Flexible PVC, Flame Retardant Sheathing Lead Free Mineral Oil resistant (75°C) |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 90/R Flexible PVC, Flame Retardant Sheathing Lead Free Hydrocarbon resistant |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 515 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com.. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 95/1 Flexible PVC, Insulation General purposes |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 0993 Flexible PVC, Insulation for High Temperatures Lead Free Insulation |
|||
Density | 1.38 - 1.43 g/cc | 0.0499 - 0.0517 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 93 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 182 Flexible PVC, Sheathing Lead Free Sheathing coaxial cable (90°) |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 79 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 86/R Flexible PVC, Flame Retardant Sheathing Hydrocarbon resistant |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 65/R Flexible PVC, Lead Free Extrusion modified with rubber |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 8050 Flexible PVC, Lead Free Pipes and profiles |
|||
Density | 1.39 - 1.43 g/cc | 0.0502 - 0.0517 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 52/C Rigid PVC, Injection Molding Electric fittings |