Fainplast Compounds GK 90/R Flexible PVC, Flame Retardant Sheathing Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds GK 90/R Flexible PVC, Flame Retardant Sheathing Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hydrocarbon resistant
Physical Properties Metric English Comments
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 91
87 - 91
ISO R 868
Tensile Strength at Break >= 18.0 MPa
>= 2610 psi
ISO R 527
Elongation at Break >= 260 %
>= 260 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 30 %
30 %
ISO 4589
Descriptive Properties Value Comments
Thermal Stability (minutes) 35
CEI 20-34/3-2