Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.63 g/cc | 0.0589 lb/in³ | DIN 53479; ASTM D792 |
Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
LATI LATAN 13 S/30 30% Glass Sphere Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | DIN 53479; ASTM D792 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
LATI Latigray 88/10-01 CX/30 PEEK Radiopaque compound based on Polyetheretherketone (PEEK). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6 GF33 FR HS L 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6 GF33 FR HS L 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WF006U PBT (Asia Pacific) LNP* THERMOCOMP* WF006U is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: UV Stabilized. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF PF00AIS PA 6 (Asia Pacific) LNP* THERMOTUF* PF00AIS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES Luriblend® POM CO GM30 TL5 30% Glass Milled Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Compos.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Vyncolit TX10916 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 51 Two-Component General Purpose Epoxy Adhesive Emerson & Cuming 51 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose epoxy adhesive. Used with a variety of catalysts. Excellent adhesion to a variety of metal, plastic.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Unitika UNILATE® 1 PC PET Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TW271F8 (PA46+PTFE)-GF40 40% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Density | 1.63 g/cc | 0.0588 lb/in³ | |
Devcon Underwater Repair Putty (UW) Epoxy Emergency Repair ProductsComments: High-performance technology for repairing, patching and rebuilding equipment in habitually wet environments, even under water. Eliminates the need for substrate t.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
A. Schulman ComAlloy Voloy® 461 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
A. Schulman ComAlloy Comtuf® 463 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | STN EN ISO 1183-1 |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Plenco 50335 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |