Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific) BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance .. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D790 |
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Density | 1.40 g/cc @Temperature 23.0 °C |
0.0506 lb/in³ @Temperature 73.4 °F |
ASTM D1505-68, method C |
Mitsubishi Hostaphan® RN, 250 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | |
Kuraray Vectran® HT 1500/300 LCP Fiber  is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | |
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 (Asia Pacific) LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXY PA 66 LNP* Thermocomp* RF006XXY is a compound based on Nylon 66 containing 30% Glass Fiber. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
Borealis FR4845 Irradiation Crosslinkable Polyethylene Compound FR4845 is an Irradiation Crosslinkable non-halogen flame retardant compound developed for the automotive wire market. Applications: FR4845 is intended for use as a 125º C rated primary insulation .. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66 Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | |
Zoltek Pyron® Oxidized Pan Staple Fiber Oxidized Pan FiberApplications include: Production of Nonwovens & Spun Yarns |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTAPROP 1540 GFC V0 H Flame Retardant Polypropylene, 20% Glass Filled PP with 20% glass fiber reinforcedFlame retardant class UL V0 and class M2 according to NL P92-507Information provided by Cossa Polimeri S.r.l. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | dry; ISO 1183 |
DSM Akulon® N24-G7 PA6-GF35 35% Glass Reinforced |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | JIS-Z-8807 |
Denka REOMER G G5379 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 329 Polyester Film, 75 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | |
DuPont Teijin Films Melinex® 426 Polyester Film, 92 Gauge Melinex® 426 is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. Melinex® 426 is chemically treated on one side for static control. The tre.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
DSM Arnite® A06 300 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | |
DuPont Teijin Films Mylar® M813 Polyester Film, 48 Gauge Mylar® M813 is a clear, pretreated base film with high gloss, low haze, and excellent processability. It is a one side pre-treated polyester designed for improved ink adhesion and may be suitable f.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFORM C 906 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Density | <= 1.40 g/cc | <= 0.0506 lb/in³ | cured 14 days @ 50% RH |
3M AC-350 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | DIN 53479 |
BASF Ultraform® FK 66003 20% Silicone Filled POM Description: Polyoxymethylene based batch with approx. 20% silicone (polysiloxane) for modifying tribological properties of thermoplastic polyoxymethylenes. Recommended concentrations of batch FK660.. |
|||
Density | 1.40 g/cc | 0.0506 lb/in³ | ISO 1183 |
BASF Ultramid® 1503-2F BK ND 3007 33% Glass Filled PA 66 (Dry) Description: Ultramid 1503-2F BK ND3007 is a 33% glass reinforced, heat stabilized injection molding PA6/6 grade. It is designed to provide enhance hydroysis resistance for under-the-hood applicatio.. |
|||
Density | <= 1.40 g/cc | <= 0.0506 lb/in³ | cured 14 days @ 50% RH |
3M AC-350 Class B-1/4 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Density | 1.40 - 1.44 g/cc | 0.0506 - 0.0520 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 84 Flexible PVC, Flame Retardant Sheathing Mineral oil resistant sheathing (80°C) |