Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
dry; ISO 1183
Water Absorption 5.7 %
5.7 %
beginning dry; ISO 62
Moisture Absorption at Equilibrium 1.7 %
1.7 %
beginning dry (23°C/50% R.H.); ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM Data; MD
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 144 MPa
20900 psi
5mm/min; ISO 527
Thermal Properties Metric English Comments
Melting Point 257 °C
495 °F
10 K/min
257 °C
495 °F
ASTM Test
Descriptive Properties Value Comments
Color Black
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding
Users viewing this material also viewed the following: