Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.36 g/cc | 0.0491 lb/in³ | |
Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 30 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can b.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | DIN 53479 |
Qualchem Danamid FGFH-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat stabilized, for long-lasting use at 120-140°C.Information provided by Qualchem Zrt. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO data |
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe a.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific) LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Styrolution Luran® 378 P G7 35% Glass Filled SAN Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183/B; ASTM D792 |
Styron CALIBREâ„¢ 5201-12 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-12 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALI.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East) LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | after drying @ 100°C |
Zircar Refractory Composites RS-DA Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | DIN 53479 |
Polyram RamTal PM8515 Acetal, High impact High impact polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Chengdu Polyster FH3303 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H3303 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | JIS-Z-8807 |
Denka VINYKON W4203 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NA40 GR30 NL PA 6.6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Eurotec® Tecolen® CP20 MF20 NL XA70 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) Information provided by BASF |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
BASF Ultramid® B3WGM24 HPX BK 2320 30% Glass/Mineral Filled PA6 (Dry) Description: Ultramid B3WGM24 HPX BK23210 is a very high productivity, 30% glass/mineral reinforced heat stabilized injection molding PA6 grade for components that require medium rigidity, excellent.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | |
3M 5200 Marine Adhesive/Sealant 3M™ Marine Adhesive/Sealant 5200 is a one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds. It has excellent adhesion to wood, gelcoat and fiberglass. It for.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Conditioned, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced 6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
BASF Ultramid® A3W2G6 BK 20560 30% Glass Filled PA66 (Conditioned) Description: Ultramid A3W2G6 BK20560 is a developmental 30% glass fiber reinforced, pigmented black, injection molding PA66/6 with high heat aging resistance.Applications: Automotive power train app.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | (Dry) |
BASF Capron® GR30 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ASTM D792 |
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry) Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Density | 1.36 g/cc | 0.0491 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |