Material Notes:
ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory Sheet Type RS-D is available in four types: TYPE RS-DA is a plastic highly moldable sheet ideally suited for forming custom geometries.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
after drying @ 100°C
1.60 g/cc
0.0578 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.490 GPa

@Temperature 600 °C,
Time 28800 sec
71.1 ksi

@Temperature 1110 °F,
Time 8.00 hour
Compressive Yield Strength 1.38 MPa
200 psi
after firing 8 hrs. at 600°C, 10% compression
Thermal Properties Metric English Comments
Specific Heat Capacity 0.250 J/g-°C
0.0598 BTU/lb-°F
Thermal Conductivity 6.57 W/m-K

@Temperature 600 °C
45.6 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Melting Point 1815 °C
3299 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Shrinkage 1.00 %

@Temperature 1000 °C
1.00 %

@Temperature 1830 °F
25.0 %

@Temperature 100 °C
25.0 %

@Temperature 212 °F
thickness shrinkage on drying
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
Other <= 1.0 %
<= 1.0 %
SiO2 10 %
10 %
Processing Properties Metric English Comments
Moisture Content 40 %
40 %
Descriptive Properties Value Comments