Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled , Nylon 66, Glass Bead Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 66
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 66 GB 30 GF 20 PA66, 20% glass fibre, 30% glass beads.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesPA 66 chemically reinforced with 20% glass fibre and with the content of 30 % glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can be changed by the ideal combination of the glass fibre and the glass beads. High surface brightness, low rolling resistance force. Manufacturing of exact parts /mainly in flat form/, throttle valves in air piping. Increased strength and tension modulus in tension due to the addition of glass fibre. Delivered in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Viscosity Measurement 0.56 - 0.63
0.56 - 0.63
Linear Mold Shrinkage 0.0056 cm/cm
0.0056 in/in
Linear Mold Shrinkage, Transverse 0.0063 cm/cm
0.0063 in/in
Melt Flow 1.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
1.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
Elongation at Break 3.5 %
3.5 %
Tensile Modulus 7.80 GPa
1130 ksi
Flexural Strength 195 MPa
28300 psi
Flexural Modulus 6.58 GPa
954 ksi
Charpy Impact Unnotched 4.50 J/cm²

@Temperature -20.0 °C
21.4 ft-lb/in²

@Temperature -4.00 °F
5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
Vicat Softening Point 240 °C
464 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 40.0 kV/mm
1020 kV/in
Comparative Tracking Index 450 V
450 V
Processing Properties Metric English Comments
Melt Temperature 260 - 290 °C
500 - 554 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi