Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Compliant with US FDA regulations.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
Cell Length 0.260 mm
0.0102 in
Mechanical Properties Metric English Comments
Hardness, Shore OO 72.5
72.5
ISO 868
Tensile Strength 0.761 MPa
110 psi
ISO 1798
Elongation at Break 85 %
85 %
Compressive Yield Strength 0.125 MPa

@Strain 25.0 %
18.1 psi

@Strain 25.0 %
ISO 7214
Tear Strength 0.669 kN/m
3.82 pli
ISO 8067
Compression Set 12 %

@Time 79200 sec,
Strain 50.0 %
12 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; ISO 7214
Thermal Properties Metric English Comments
Thermal Conductivity 0.0323 W/m-K
0.224 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
0.0369 W/m-K
0.256 BTU-in/hr-ft²-°F
mean temp of 50°C; ISO 8301
0.0416 W/m-K
0.289 BTU-in/hr-ft²-°F
mean temp of 83°C; ISO 8301
Maximum Service Temperature, Air 155 °C
311 °F
Descriptive Properties Value Comments
Flammability Heat Release: FAR/CS 25.853
Pass at 1/2 in
Radiant Heat Panel: FAR 25.856
Pass at 1/8, 1/2, and 1 in
Smoke Density: ABD0031
Pass at 1/2 in
Smoke Density: FAR/CS 25.853
Pass at 1/2 in
Toxic Gas Emission: ABD0031
Pass at 1/2 in
Vertical Burner (60 sec): FAR/CS 25.853
Pass at 1 in