Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
Zotefoams ZOTEK® F 40 HT PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | |
Hexcel® HexWeb® HRH-36 - 1/8 - 2.5 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | |
Hexcel® HexWeb® HRH-36/OX - 3/16 - 2.5 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | |
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.5 Aramid Honeycomb Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | |
Hexcel® HexWeb® HRP/F35 - 2.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | |
Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Density | 0.0400 - 0.0600 g/cc | 0.00145 - 0.00217 lb/in³ | ISO 845-88 |
Eurofoam Evacell EVA 50/S EVA + NR Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.0400 - 0.0500 g/cc | 0.00145 - 0.00181 lb/in³ | ISO 845-88 |
Eurofoam Polycell PLZ 45 Polyethylene Foam Information provided by Eurofoam s.r.l. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | DIN 53420 |
Dow STRANDFOAM™ EA 1000 Polypropylene Foam STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 8015 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9230 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9435 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | ISO 845 |
BASF Neopolen® P 8220 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Density | 0.0400 - 0.0800 g/cc | 0.00145 - 0.00289 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 522F Expandable Polystyrene GENERAL: PENTFOAM "522F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V.. |
|||
Density | 0.0400 - 0.0800 g/cc | 0.00145 - 0.00289 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene GENERAL: PENTFOAM "526W" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT.APPLICATIONS: PENTFOAM "526W" IS PARTICULARLY WELL SUITED FOR THE MANUFA.. |
|||
Density | 0.0400 g/cc | 0.00145 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® C70.40 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |