Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 0.758 MPa | >= 110 psi | |
Parker Chomerics Tecknit Teckfip™ FIP-C Formed in Place Conductive Elastomer Description: This compound is an all round high performance compound, and is very similar to a Consil C molded or extruded elastomer. It has been traditionally used for telecommunications base stati.. |
|||
Tensile Strength | 0.758 MPa | 110 psi | Die A; ASTM D412 |
Monmouth Rubber & Plastics Durafoamâ„¢ C44 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 0.758 MPa | >= 110 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Tensile Strength | >= 0.758 MPa | >= 110 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Tensile Strength | 0.761 MPa | 110 psi | ISO 1798 |
Zotefoams ZOTEK® F 40 HT PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |