Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.125 MPa @Strain 25.0 % |
18.1 psi @Strain 25.0 % |
ISO 7214 |
Zotefoams ZOTEK® F 40 HT PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |