Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amco Amalloy® B9714 Polymer Alloy

Category Polymer , Thermoplastic
Manufacturer Amco Plastic Materials
Trade Name Amalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco Amalloy® B9714 Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amco Amalloy B9714 is a clear performance copolymer with exceptional clarity and toughness.High elongation before breakage, good melt Flow.Information provided by Amco Plastic Materials.
Physical Properties Metric English Comments
Melt Flow 6.3 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.3 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 72
72
ASTM D785
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 106 %
106 %
ASTM D638
Tensile Modulus 1.74 GPa
253 ksi
ASTM D638
Flexural Strength 39.82 MPa
5775 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 0.278 J/cm
0.520 ft-lb/in
ASTM D256
Optical Properties Metric English Comments
Haze 1.4 %

@Thickness 2.54 mm
1.4 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 90.7 %

@Thickness 2.54 mm
90.7 %

@Thickness 0.100 in
ASTM D1003