Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 12.9 g/cc | 0.466 lb/in³ | |
Wieland 1416 Wilaform Gold Hard yellow gold alloy with good extensibility. By grain stabilization particularly suitable for the production of chains or poured parts.Applications: casting, chains, laminar decoration, pipesDen.. |
|||
Density | 12.9 g/cc | 0.466 lb/in³ | |
China Tungsten YT5 Tungsten Carbide for Cutting Tools Best strength and height impact & shock resistance among W-Co-Ti alloys but wear resistance comparatively lower. Rough turning, rough planning and half precision planning of carbon steel and alloy s.. |
|||
Density | 12.9 g/cc | 0.466 lb/in³ | |
China Tungsten YW2 Tungsten Carbide for Cutting Tools Wear resistance second to YW1 yet strength comparatively higher and resistant to high impact load. Roughing and medium machining of ordinary steel cst irons as well as refractory steel, manganese st.. |
|||
Density | 12.9 g/cc | 0.466 lb/in³ | |
China Tungsten YW2A Tungsten Carbide for Cutting Tools High red hardness and high strength in use, resisting high impact load, A good grade for general purposes, Machining and medium machine of cast irons and problem materials such as refractory steel, .. |