Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 840 °C | 1540 °F | |
Wieland 1416 Wilaform Gold Hard yellow gold alloy with good extensibility. By grain stabilization particularly suitable for the production of chains or poured parts.Applications: casting, chains, laminar decoration, pipesDen.. |
|||
Solidus | 840 °C | 1540 °F | |
Wieland 1910 Wilaform Gold Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental |
|||
Solidus | 835 °C | 1540 °F | |
Williams Advanced Alloys Wambraze™ WB845 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |