Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 840 - 870 °C | 1540 - 1600 °F | |
Wieland 1416 Wilaform Gold Hard yellow gold alloy with good extensibility. By grain stabilization particularly suitable for the production of chains or poured parts.Applications: casting, chains, laminar decoration, pipesDen.. |
|||
Melting Point | 840 - 860 °C | 1540 - 1580 °F | |
Wieland 1910 Wilaform Gold Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental |
|||
Melting Point | 840 °C | 1540 °F | |
Goodfellow Copper 85/Silicon 15 Alloy Information provided by Goodfellow. |