Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin

Category Polymer , Film , Thermoplastic , Fluoropolymer , ETFE/ECTFE , ECTFE Fluoropolymer
Manufacturer Westlake Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.1 MPa
4940 psi
ASTM D882
Elongation at Break 220 %
220 %
ASTM D882
Tensile Modulus 1.96 GPa
284 ksi
ASTM D882
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Tear Strength 198 kN/m
1130 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
DSC
Maximum Service Temperature, Air 150 °C
302 °F
Continuous Use
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ASTM D648
Flammability, UL94 V-0
V-0
VTM-0
Oxygen Index 60 %
60 %
ASTM D2863
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+16 ohm
>= 1.00e+16 ohm
ASTM D257
Dielectric Constant 2.56

@Frequency 1000 Hz
2.56

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 105 kV/mm

@Thickness 0.0762 mm
2670 kV/in

@Thickness 0.00300 in
ASTM D149
Dissipation Factor 0.0025 - 0.0050

@Frequency 1000 Hz
0.0025 - 0.0050

@Frequency 1000 Hz
ASTM D150
Users viewing this material also viewed the following: